Fabrication reference

Weld Defects: Causes and Fixes

Porosity, undercut, spatter and lack of fusion are the four weld defects welders search for most. For each one, this guide lists the likely causes, most common first, with the fix for each cause.

What causes porosity in welding?

Porosity is small round holes in or on the bead, left by gas trapped as the weld froze. The most common cause is dirty metal (rust, oil, paint, moisture or mill scale), followed by a gas flow or gas coverage problem.

Porosity: causes and fixes, most common cause first
CauseFix
Dirty base metal: rust, oil, paint, moisture or mill scaleClean the joint back to bright metal and keep it dry
Gas flow too low or too high, or a leak in the gas lineSet gas flow to the chart and check hoses/fittings for leaks
Draft or wind blowing the shielding gas awayScreen the weld from wind (close doors, use a tent)
Damp or damaged electrodes / flux-cored wireDry and store consumables per the datasheet
Arc too long, or wrong / no shielding gasShorten the arc and confirm the correct gas

Shows up in: MIG, TIG, flux-core and stick.

What causes undercut in welding?

Undercut is a groove melted into the base metal along the edge of the weld and left unfilled. It usually comes from too much current or voltage, too long an arc, or traveling too fast.

Undercut: causes and fixes, most common cause first
CauseFix
Current or voltage too highLower the current
Arc too longShorten the arc
Travel speed too fastSlow the travel
Wrong torch / electrode angleHold the torch at about 45°, splitting the corner
Weave too wide with no pause at the toesPause briefly at each toe to fill it

Shows up in: MIG, stick and flux-core.

What causes weld spatter?

Spatter is beads of metal thrown onto the plate around the weld. It is mostly cosmetic, but it slows clean-up. The usual causes are voltage that does not suit the wire and amps, too much CO2 in the shielding gas, dirty metal and too long a stick-out.

Excessive spatter: causes and fixes, most common cause first
CauseFix
Voltage too low or too high for the wire and ampsTune the voltage to the wire and amperage
Too much CO2 in the shielding gasUse a higher-argon mix (for example C25, which is 75% argon and 25% CO2) for less spatter
Dirty or rusty base metalClean the metal
Long stick-out / contact-tip-to-work distanceReduce the stick-out
Wrong polarity or damp fluxConfirm polarity and dry the consumables

Shows up in: MIG and flux-core.

What is lack of fusion in welding?

Lack of fusion is weld metal that sits on the base metal, or on the run before it, without melting into it. It usually comes from too little heat, traveling too fast, or pointing the arc at the pool and not at the joint face.

Lack of fusion: causes and fixes, most common cause first
CauseFix
Heat input too lowRaise the current / heat input
Travel too fast, or the puddle running ahead of the arcSlow down so the pool wets the sidewalls
Arc aimed at the pool, not the fusion faceDirect the arc at the leading edge and the fusion line
Dirty or oxidized surfaces between passesClean between passes
Poor access or a joint angle that hides the sidewallImprove access and the work angle

Shows up in: MIG and flux-core on cold settings.

Other weld faults

Twelve more faults, with what each one looks like. The causes and fixes for these are in the free Weld Fault Finder in Fabora Steel Tools.

On the weld

Weld faults and what each one looks like
FaultWhat it looks like
Lack of penetrationThe weld does not reach the joint root, leaving the root unfilled.
Overlap / cold lapWeld metal spilled over the base metal at the toe without fusing to it.
Burn-throughThe arc melts fully through, leaving a hole or a sagging, collapsed root.
CrackingA split in the weld or heat-affected zone: hot (while cooling) or cold (hours later).
Slag inclusionNon-metallic slag trapped in the weld, often as a dark line or pockets along a bead edge or between runs.
Distortion / warpingThe part pulls out of shape as the weld cools: angular twist, bowing, or shrinkage across the joint.
Magnetic arc blowThe arc wanders or is pushed to one side (usually near ends and edges), causing uneven fusion, porosity and spatter.

At the machine

Machine faults and what each one looks like
FaultWhat it looks like
Bird-nestingThe wire bunches up and tangles at the drive rolls instead of feeding up the torch.
BurnbackThe wire melts back and fuses to the contact tip, so the wire stops feeding.
Wrong polarity (gasless wire)Gasless flux-cored wire spits, spatters heavily and leaves a lumpy bead sitting on top.
Thermal cut-outThe welder stops and a warning light comes on. It will not weld again until it has cooled.
Supply tripsThe breaker trips or the fuse blows when you strike an arc or turn the amps up.

In the Steel Tools app

The Weld Fault Finder in Fabora Steel Tools is free and works with no signal:

  • all 16 faults: 11 on the weld and 5 at the machine
  • pick what you can see in plain words, such as "Holes or bubbles in the weld"
  • the likely causes, most common first, with the fix for each one
  • a drawing of every fault

Steel Tools is free to download for iPhone and Android, and the Weld Fault Finder is one of its free tools.

Weld defect questions

How do you prevent porosity in welding?

Clean the joint back to bright metal and keep it dry. Set the gas flow to the chart and check hoses and fittings for leaks. Screen the weld from wind. Keep electrodes and flux-cored wire dry, keep the arc short and confirm the gas is the right one.

What can cure undercut in welding?

Lower the current, shorten the arc and slow the travel. Hold the torch at about 45 degrees so it splits the corner, and pause briefly at each toe of a weave to fill it.

How do you avoid lack of fusion?

Raise the current or heat input and slow down so the pool wets the sidewalls. Point the arc at the leading edge and the fusion line, clean between passes, and improve access and the work angle.

What are the 7 common welding defects?

Lists vary from source to source. The ones named most often are porosity, undercut, lack of fusion, lack of penetration, cracking, slag inclusion and spatter. The Weld Fault Finder in Fabora Steel Tools covers those and nine more, including five machine faults.

What is the maximum acceptable depth of undercut?

It depends on the code the job is built to, such as AWS D1.1 or ISO 5817, and on how the joint is loaded. Check the acceptance table in that code or the job specification. This guide is general shop guidance and does not replace it.

Which welding processes get porosity?

All the common arc processes: MIG, TIG, flux-core and stick.

Last updated: November 16, 2026. Causes and fixes are general shop guidance, not a substitute for inspection to the applicable acceptance standard (for example AWS D1.1 or ISO 5817).

Fabora Steel Tools

Weld Fault Finder in Fabora Steel Tools

The Weld Fault Finder in Fabora Steel Tools is free and works with no signal.

Works offlineFree tool16 faults